Flocking Paste

Feb 25, 2021 Leave a message

Cowint TDS of Flocking Paste

 

DONGGUAN COWINT NEW MATERIAL TECHNOLOGY CO.,LTD

No.2,West Industrial Road of Jiaoli,Zhongtang Town,Dongguan  

Tel: +86-769-88882603   Web:www.cowint2.com                 

mail: info@cowint.com

 

 

1. Need products:

   

CTS-F620 Flocking Paste

   

Fixer:CT-31

 

 

2.Used method:

 

98% Flocking paste + 2% additives;

 The printing process of the test piece: the first

time of flocking pulp primer → drying → the

second time of printing, leaving the pulp and flocking

→ 145°C overheating for 90S → finished product.

      

 

2. 
The printing process:

  98% Flocking paste + 2% additives;

Flocking pulp first time → blow-drying → printing

for the second time leaving pulp and flocking → natural

drying or drying → finished product

 

 

3. Attention:

1.Please use up the flocking pulp with additives within 3-4 hours to avoid instability;

② The flocking pulp contains a special self-crosslinking polymer, which can autocatalyze during drying and processing. It can reach the ideal fastness after being placed at room temperature for 48 hours;

③ For fabrics with high elasticity (or coarse fabric), it is best to use flocking pulp as a primer first, and then stamp the flocking pulp once after half-drying. (Do not blow dry) immediately flock (flock) to improve the three-dimensional feeling of flocking (flock) And fastness.

④ Make sure that the printing is completely dry during testing, otherwise it will affect the test results.

⑤ 140-160°C, 90S: 2.2m drying tunnel 10 turns.

3